AWS ENiCrMo-4 vs. Nickel Beryllium 360
Both AWS ENiCrMo-4 and nickel beryllium 360 are nickel alloys. There are 15 material properties with values for both materials. Properties with values for just one material (14, in this case) are not shown.
For each property being compared, the top bar is AWS ENiCrMo-4 and the bottom bar is nickel beryllium 360.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 220 | |
200 |
Elongation at Break, % | 28 | |
1.0 to 30 |
Poisson's Ratio | 0.29 | |
0.3 |
Shear Modulus, GPa | 84 | |
77 |
Tensile Strength: Ultimate (UTS), MPa | 790 | |
780 to 1860 |
Thermal Properties
Melting Completion (Liquidus), °C | 1590 | |
1330 |
Melting Onset (Solidus), °C | 1530 | |
1200 |
Specific Heat Capacity, J/kg-K | 410 | |
460 |
Thermal Expansion, µm/m-K | 12 | |
14 |
Otherwise Unclassified Properties
Density, g/cm3 | 9.0 | |
8.3 |
Common Calculations
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 22 | |
24 |
Strength to Weight: Axial, points | 24 | |
26 to 62 |
Strength to Weight: Bending, points | 21 | |
23 to 41 |
Thermal Shock Resistance, points | 22 | |
19 to 46 |