Both ABS and PMP are thermoplastics. There are 13 material properties with values for both materials. Properties with values for just one material (13, in this case) are not shown.

For each property being compared, the top bar is ABS and the bottom bar is PMP.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 2.0 to 2.6
1.1
Elongation at Break, % 3.5 to 50
30
Impact Strength: Notched Izod, J/m 70 to 370
130
Tensile Strength: Ultimate (UTS), MPa 37 to 110
24

Thermal Properties

Thermal Expansion, µm/m-K 81 to 95
120

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz 3.1 to 3.2
2.1
Dielectric Strength (Breakdown Potential), kV/mm 15 to 16
28

Otherwise Unclassified Properties

Density, g/cm3 1.0 to 1.4
0.83

Common Calculations

Stiffness to Weight: Axial, points 0.79 to 1.4
0.74
Stiffness to Weight: Bending, points 30 to 44
41
Strength to Weight: Axial, points 10 to 22
8.0
Strength to Weight: Bending, points 24 to 37
22
Thermal Shock Resistance, points 11 to 50
13