Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 2.6 | |
1.6 to 2.3 |
Elongation at Break, % | 6.0 | |
110 to 120 |
Tensile Strength: Ultimate (UTS), MPa | 55 | |
45 to 60 |
Thermal Properties
Specific Heat Capacity, J/kg-K | 1300 | |
1510 |
Thermal Conductivity, W/m-K | 0.18 | |
0.23 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 Hz | 3.7 | |
3.9 to 12 |
Otherwise Unclassified Properties
Density, g/cm3 | 1.1 | |
1.1 |
Common Calculations
Stiffness to Weight: Axial, points | 1.3 | |
0.78 to 1.1 |
Stiffness to Weight: Bending, points | 43 | |
34 to 39 |
Strength to Weight: Axial, points | 14 | |
11 to 15 |
Strength to Weight: Bending, points | 30 | |
25 to 30 |
Thermal Diffusivity, mm2/s | 0.13 | |
0.13 |