MakeItFrom.com
Menu (ESC)

Annealed 88-silver 12-tin-oxide vs. Annealed 92-silver 8-tin-oxide

Both annealed 88-silver 12-tin-oxide and annealed 92-silver 8-tin-oxide are otherwise unclassified metals. Both are furnished in the annealed condition.

For each property being compared, the top bar is annealed 88-silver 12-tin-oxide and the bottom bar is annealed 92-silver 8-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 86
80
Elongation at Break, % 37
32
Resilience: Ultimate (Unit Rupture Work), MJ/m3 70
62
Shear Strength, MPa 150
150
Tensile Strength: Ultimate (UTS), MPa 230
230
Tensile Strength: Yield (Proof), MPa 110
120