Annealed 92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while annealed SAE-AISI 9310 belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.
For each property being compared, the top bar is annealed 92-silver 8-tin-oxide and the bottom bar is annealed SAE-AISI 9310.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 80 | |
7.7 |
Elongation at Break, % | 32 | |
17 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 | |
120 |
Shear Strength, MPa | 150 | |
510 |
Tensile Strength: Ultimate (UTS), MPa | 230 | |
820 |
Tensile Strength: Yield (Proof), MPa | 120 | |
450 |