MakeItFrom.com
Menu (ESC)

Annealed 92-silver 8-tin-oxide vs. Annealed K93603 Alloy

Annealed 92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while annealed K93603 alloy belongs to the iron alloys. There are 2 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.

For each property being compared, the top bar is annealed 92-silver 8-tin-oxide and the bottom bar is annealed K93603 alloy.

Metric UnitsUS Customary Units

Material Properties

Tensile Strength: Ultimate (UTS), MPa 230
490
Tensile Strength: Yield (Proof), MPa 120
290