Automotive grey cast iron belongs to the iron alloys classification, while grade 24 titanium belongs to the titanium alloys. There are 26 material properties with values for both materials. Properties with values for just one material (6, in this case) are not shown.

For each property being compared, the top bar is automotive grey cast iron and the bottom bar is grade 24 titanium.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 180
110
Elongation at Break, % 9.6 to 14
11
Poisson's Ratio 0.29
0.32
Shear Modulus, GPa 69 to 70
40
Tensile Strength: Ultimate (UTS), MPa 140 to 290
1010
Tensile Strength: Yield (Proof), MPa 94 to 200
940

Thermal Properties

Latent Heat of Fusion, J/g 260 to 280
410
Melting Completion (Liquidus), °C 1380 to 1390
1610
Melting Onset (Solidus), °C 1340 to 1350
1560
Specific Heat Capacity, J/kg-K 490
560
Thermal Conductivity, W/m-K 41 to 43
7.1
Thermal Expansion, µm/m-K 12 to 14
9.6

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.4 to 7.6
1.0
Electrical Conductivity: Equal Weight (Specific), % IACS 8.8 to 9.1
2.0

Otherwise Unclassified Properties

Density, g/cm3 7.5 to 7.6
4.5
Embodied Carbon, kg CO2/kg material 1.5 to 1.7
43
Embodied Energy, MJ/kg 21 to 24
710
Embodied Water, L/kg 44 to 51
310

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 18 to 25
110
Resilience: Unit (Modulus of Resilience), kJ/m3 25 to 110
4160
Stiffness to Weight: Axial, points 13
13
Stiffness to Weight: Bending, points 25
35
Strength to Weight: Axial, points 5.2 to 11
63
Strength to Weight: Bending, points 8.0 to 13
50
Thermal Diffusivity, mm2/s 11 to 12
2.9
Thermal Shock Resistance, points 4.2 to 8.6
72