Automotive grey cast iron belongs to the iron alloys classification, while R30016 cobalt belongs to the cobalt alloys. There are 26 material properties with values for both materials. Properties with values for just one material (8, in this case) are not shown.

For each property being compared, the top bar is automotive grey cast iron and the bottom bar is R30016 cobalt.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 180
220
Elongation at Break, % 9.6 to 14
8.4
Poisson's Ratio 0.29
0.28
Shear Modulus, GPa 69 to 70
85
Tensile Strength: Ultimate (UTS), MPa 140 to 290
1010
Tensile Strength: Yield (Proof), MPa 94 to 200
580

Thermal Properties

Latent Heat of Fusion, J/g 260 to 280
320
Melting Completion (Liquidus), °C 1380 to 1390
1360
Melting Onset (Solidus), °C 1340 to 1350
1270
Specific Heat Capacity, J/kg-K 490
450
Thermal Conductivity, W/m-K 41 to 43
15
Thermal Expansion, µm/m-K 12 to 14
14

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.4 to 7.6
1.9
Electrical Conductivity: Equal Weight (Specific), % IACS 8.8 to 9.1
2.0

Otherwise Unclassified Properties

Density, g/cm3 7.5 to 7.6
8.5
Embodied Carbon, kg CO2/kg material 1.5 to 1.7
7.7
Embodied Energy, MJ/kg 21 to 24
110
Embodied Water, L/kg 44 to 51
500

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 18 to 25
72
Resilience: Unit (Modulus of Resilience), kJ/m3 25 to 110
770
Stiffness to Weight: Axial, points 13
14
Stiffness to Weight: Bending, points 25
24
Strength to Weight: Axial, points 5.2 to 11
33
Strength to Weight: Bending, points 8.0 to 13
26
Thermal Diffusivity, mm2/s 11 to 12
3.9
Thermal Shock Resistance, points 4.2 to 8.6
24