Both automotive malleable cast iron and ASTM A216 cast steel are iron alloys. There are 27 material properties with values for both materials. Properties with values for just one material (4, in this case) are not shown.

For each property being compared, the top bar is automotive malleable cast iron and the bottom bar is ASTM A216 cast steel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 180
190
Elongation at Break, % 1.0 to 10
25 to 27
Poisson's Ratio 0.29
0.29
Shear Modulus, GPa 70
72
Tensile Strength: Ultimate (UTS), MPa 350 to 720
500 to 570
Tensile Strength: Yield (Proof), MPa 220 to 590
230 to 310

Thermal Properties

Latent Heat of Fusion, J/g 260
250
Melting Completion (Liquidus), °C 1410
1450 to 1460
Melting Onset (Solidus), °C 1370
1410
Specific Heat Capacity, J/kg-K 480
470
Thermal Conductivity, W/m-K 41
49 to 52
Thermal Expansion, µm/m-K 14
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.4
7.1 to 7.2
Electrical Conductivity: Equal Weight (Specific), % IACS 8.7
8.2 to 8.3

Otherwise Unclassified Properties

Base Metal Price, % relative 1.9
1.8
Density, g/cm3 7.6
7.8
Embodied Carbon, kg CO2/kg material 1.5
1.4
Embodied Energy, MJ/kg 20
18
Embodied Water, L/kg 45
45

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 6.8 to 30
110 to 120
Resilience: Unit (Modulus of Resilience), kJ/m3 130 to 950
140 to 250
Stiffness to Weight: Axial, points 13
13
Stiffness to Weight: Bending, points 25
24
Strength to Weight: Axial, points 13 to 26
18 to 20
Strength to Weight: Bending, points 14 to 24
18 to 20
Thermal Diffusivity, mm2/s 11
13 to 14
Thermal Shock Resistance, points 9.9 to 21
16 to 18