CAB vs. UP
CAB belongs to the thermoplastics classification, while UP belongs to the thermoset plastics. There are 11 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is CAB and the bottom bar is UP.
Metric UnitsUS Customary Units
Mechanical Properties
Elongation at Break, % | 50 to 55 | |
1.0 |
Tensile Strength: Ultimate (UTS), MPa | 20 to 50 | |
30 |
Thermal Properties
Glass Transition Temperature, °C | 140 | |
60 |
Specific Heat Capacity, J/kg-K | 1460 | |
1200 |
Thermal Conductivity, W/m-K | 0.25 | |
0.7 |
Thermal Expansion, µm/m-K | 14 | |
3.0 |
Otherwise Unclassified Properties
Density, g/cm3 | 1.2 | |
2.0 |
Limiting Oxygen Index (LOI), % | 18 | |
20 |
Common Calculations
Strength to Weight: Axial, points | 4.8 to 12 | |
4.2 |
Strength to Weight: Bending, points | 14 to 25 | |
11 |
Thermal Diffusivity, mm2/s | 0.14 to 0.15 | |
0.29 |