CSM Rubber vs. Thermoplastic PI
CSM rubber belongs to the thermoset elastomers (rubber) classification, while thermoplastic PI belongs to the thermoplastics. There are 7 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.
For each property being compared, the top bar is CSM rubber and the bottom bar is thermoplastic PI.
Metric UnitsUS Customary Units
Material Properties
Density, g/cm3 | 1.2 | |
1.4 to 1.5 |
Elongation at Break, % | 400 | |
1.8 to 7.5 |
Glass Transition Temperature, °C | 0 | |
260 |
Limiting Oxygen Index (LOI), % | 25 | |
35 |
Strength to Weight: Axial, points | 2.1 | |
22 to 42 |
Strength to Weight: Bending, points | 8.0 | |
36 to 57 |
Tensile Strength: Ultimate (UTS), MPa | 9.0 | |
110 to 220 |