Class 2 Tungsten vs. 85-silver 15-nickel
Both class 2 tungsten and 85-silver 15-nickel are otherwise unclassified metals. There are 15 material properties with values for both materials. Properties with values for just one material (12, in this case) are not shown.
For each property being compared, the top bar is class 2 tungsten and the bottom bar is 85-silver 15-nickel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 260 | |
88 |
Poisson's Ratio | 0.28 | |
0.36 |
Shear Modulus, GPa | 100 | |
32 |
Tensile Strength: Ultimate (UTS), MPa | 860 | |
260 to 470 |
Thermal Properties
Latent Heat of Fusion, J/g | 160 | |
140 |
Specific Heat Capacity, J/kg-K | 120 | |
270 |
Thermal Expansion, µm/m-K | 4.6 | |
18 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 13 | |
86 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 7.8 | |
75 |
Otherwise Unclassified Properties
Density, g/cm3 | 15 | |
10 |
Common Calculations
Stiffness to Weight: Axial, points | 9.6 | |
4.8 |
Stiffness to Weight: Bending, points | 14 | |
14 |
Strength to Weight: Axial, points | 16 | |
7.1 to 13 |
Strength to Weight: Bending, points | 13 | |
8.9 to 13 |
Thermal Shock Resistance, points | 52 | |
12 to 21 |
Alloy Composition
Nickel (Ni), % | 0 | |
13.8 to 16 |
Silver (Ag), % | 0 | |
84 to 86 |
Tungsten (W), % | 92.5 | |
0 |
Residuals, % | 0 | |
0 to 0.2 |