Material Properties

Electrical Conductivity: Equal Volume, % IACS 18
84
Elongation at Break, % 23
9.0
Resilience: Ultimate (Unit Rupture Work), MJ/m3 110
24
Shear Strength, MPa 340
160
Tensile Strength: Ultimate (UTS), MPa 540
280
Tensile Strength: Yield (Proof), MPa 370
260