Cold Worked R60901 Alloy vs. Work Hardened ASTM B522 Class II

Both cold worked R60901 alloy and work hardened ASTM B522 class II are otherwise unclassified metals. Both are furnished in the cold worked (strain hardened) condition. There are 18 material properties with values for both materials. Properties with values for just one material (8, in this case) are not shown. Please note that the two materials have significantly dissimilar densities. This means that additional care is required when interpreting the data, because some material properties are based on units of mass, while others are based on units of area or volume.

For each property being compared, the top bar is cold worked R60901 alloy and the bottom bar is work hardened ASTM B522 class II.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 98
96
Elongation at Break, % 17
1.1
Poisson's Ratio 0.34
0.41
Shear Modulus, GPa 37
34
Tensile Strength: Ultimate (UTS), MPa 580
490
Tensile Strength: Yield (Proof), MPa 390
210

Thermal Properties

Latent Heat of Fusion, J/g 250
77
Melting Completion (Liquidus), °C 1870
1030
Specific Heat Capacity, J/kg-K 270
160
Thermal Expansion, µm/m-K 6.3
15

Otherwise Unclassified Properties

Density, g/cm3 6.6
17

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 88
4.4
Resilience: Unit (Modulus of Resilience), kJ/m3 760
230
Stiffness to Weight: Axial, points 8.3
3.1
Stiffness to Weight: Bending, points 23
8.9
Strength to Weight: Axial, points 25
7.8
Strength to Weight: Bending, points 24
8.0
Thermal Shock Resistance, points 67
24

Alloy Composition

Gold (Au), % 0
68.5 to 69.5
Niobium (Nb), % 2.4 to 2.8
0
Platinum (Pt), % 0
5.5 to 6.5
Silver (Ag), % 0
24.5 to 25.5
Sulfur (S), % 0
0 to 0.010
Zirconium (Zr), % 96.8 to 97.5
0
Residuals, % 0
0 to 0.26