DAP vs. NEMA Laminate
Both DAP and NEMA laminate are thermoset plastics. There are 9 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is DAP and the bottom bar is NEMA laminate.
Metric UnitsUS Customary Units
Material Properties
Compressive (Crushing) Strength, MPa | 150 | |
190 to 360 |
Density, g/cm3 | 1.7 | |
1.3 to 1.9 |
Dielectric Strength (Breakdown Potential), kV/mm | 40 | |
12 to 21 |
Flexural Strength, MPa | 62 | |
87 to 340 |
Impact Strength: Notched Izod, J/m | 14 | |
20 to 430 |
Strength to Weight: Axial, points | 4.5 | |
8.3 to 40 |
Strength to Weight: Bending, points | 12 | |
17 to 50 |
Tensile Strength: Ultimate (UTS), MPa | 28 | |
55 to 260 |
Thermal Expansion, µm/m-K | 25 | |
9.0 to 20 |