EN 1.1127 Steel vs. ASTM A285 Carbon Steel
Both EN 1.1127 steel and ASTM A285 carbon steel are iron alloys.
For each property being compared, the top bar is EN 1.1127 steel and the bottom bar is ASTM A285 carbon steel.
Metric UnitsUS Customary Units
Mechanical Properties
Brinell Hardness | 190 to 230 | |
110 to 130 |
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 14 to 25 | |
30 to 34 |
Fatigue Strength, MPa | 280 to 370 | |
150 to 180 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
73 |
Shear Strength, MPa | 420 to 480 | |
250 to 290 |
Tensile Strength: Ultimate (UTS), MPa | 660 to 790 | |
380 to 450 |
Tensile Strength: Yield (Proof), MPa | 410 to 580 | |
190 to 230 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
250 |
Maximum Temperature: Mechanical, °C | 400 | |
400 |
Melting Completion (Liquidus), °C | 1460 | |
1470 |
Melting Onset (Solidus), °C | 1410 | |
1420 to 1430 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 49 | |
53 |
Thermal Expansion, µm/m-K | 12 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.3 | |
7.0 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.4 | |
8.0 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 2.1 | |
1.8 |
Density, g/cm3 | 7.8 | |
7.9 |
Embodied Carbon, kg CO2/kg material | 1.5 | |
1.4 |
Embodied Energy, MJ/kg | 19 | |
18 |
Embodied Water, L/kg | 49 | |
46 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 90 to 140 | |
110 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 440 to 880 | |
94 to 150 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 23 to 28 | |
13 to 16 |
Strength to Weight: Bending, points | 22 to 24 | |
15 to 17 |
Thermal Diffusivity, mm2/s | 13 | |
14 |
Thermal Shock Resistance, points | 21 to 25 | |
12 to 14 |