EN 1.1151 Steel vs. ASTM A285 Carbon Steel
Both EN 1.1151 steel and ASTM A285 carbon steel are iron alloys.
For each property being compared, the top bar is EN 1.1151 steel and the bottom bar is ASTM A285 carbon steel.
Metric UnitsUS Customary Units
Mechanical Properties
Brinell Hardness | 130 to 150 | |
110 to 130 |
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 21 to 26 | |
30 to 34 |
Fatigue Strength, MPa | 180 to 240 | |
150 to 180 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
73 |
Shear Strength, MPa | 300 to 330 | |
250 to 290 |
Tensile Strength: Ultimate (UTS), MPa | 460 to 520 | |
380 to 450 |
Tensile Strength: Yield (Proof), MPa | 240 to 340 | |
190 to 230 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
250 |
Maximum Temperature: Mechanical, °C | 400 | |
400 |
Melting Completion (Liquidus), °C | 1460 | |
1470 |
Melting Onset (Solidus), °C | 1420 | |
1420 to 1430 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 50 | |
53 |
Thermal Expansion, µm/m-K | 12 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.1 | |
7.0 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.2 | |
8.0 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 2.1 | |
1.8 |
Density, g/cm3 | 7.8 | |
7.9 |
Embodied Carbon, kg CO2/kg material | 1.4 | |
1.4 |
Embodied Energy, MJ/kg | 19 | |
18 |
Embodied Water, L/kg | 47 | |
46 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 98 to 100 | |
110 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 160 to 310 | |
94 to 150 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 16 to 18 | |
13 to 16 |
Strength to Weight: Bending, points | 17 to 18 | |
15 to 17 |
Thermal Diffusivity, mm2/s | 13 | |
14 |
Thermal Shock Resistance, points | 15 to 16 | |
12 to 14 |