EN 1.5682 steel belongs to the iron alloys classification, while N07041 nickel belongs to the nickel alloys. There are 17 material properties with values for both materials. Properties with values for just one material (15, in this case) are not shown.

For each property being compared, the top bar is EN 1.5682 steel and the bottom bar is N07041 nickel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
220
Elongation at Break, % 21
14
Fatigue Strength, MPa 400
540
Shear Strength, MPa 480
850
Tensile Strength: Ultimate (UTS), MPa 770
1400
Tensile Strength: Yield (Proof), MPa 570
1050

Thermal Properties

Melting Onset (Solidus), °C 1410
1320
Specific Heat Capacity, J/kg-K 470
450
Thermal Expansion, µm/m-K 13
12

Otherwise Unclassified Properties

Density, g/cm3 7.9
8.2

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 150
180
Resilience: Unit (Modulus of Resilience), kJ/m3 870
2510
Stiffness to Weight: Axial, points 13
15
Stiffness to Weight: Bending, points 24
25
Strength to Weight: Axial, points 27
47
Strength to Weight: Bending, points 23
34
Thermal Shock Resistance, points 23