EN 1.6553 Steel vs. 92-silver 8-tin-oxide
EN 1.6553 steel belongs to the iron alloys classification, while 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (27, in this case) are not shown.
For each property being compared, the top bar is EN 1.6553 steel and the bottom bar is 92-silver 8-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 7.5 | |
76 to 80 |
Elongation at Break, % | 19 to 21 | |
32 to 34 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 130 to 150 | |
62 to 110 |
Tensile Strength: Ultimate (UTS), MPa | 710 to 800 | |
230 to 320 |
Tensile Strength: Yield (Proof), MPa | 470 to 670 | |
120 to 300 |