EN 1.7016 Steel vs. N07041 Nickel
EN 1.7016 steel belongs to the iron alloys classification, while N07041 nickel belongs to the nickel alloys. There are 13 material properties with values for both materials. Properties with values for just one material (18, in this case) are not shown.
For each property being compared, the top bar is EN 1.7016 steel and the bottom bar is N07041 nickel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
220 |
Tensile Strength: Ultimate (UTS), MPa | 450 to 1390 | |
1400 |
Thermal Properties
Melting Onset (Solidus), °C | 1420 | |
1320 |
Specific Heat Capacity, J/kg-K | 470 | |
450 |
Thermal Conductivity, W/m-K | 45 | |
11 |
Thermal Expansion, µm/m-K | 13 | |
12 |
Otherwise Unclassified Properties
Density, g/cm3 | 7.8 | |
8.2 |
Common Calculations
Stiffness to Weight: Axial, points | 13 | |
15 |
Stiffness to Weight: Bending, points | 24 | |
25 |
Strength to Weight: Axial, points | 16 to 49 | |
47 |
Strength to Weight: Bending, points | 17 to 35 | |
34 |
Thermal Diffusivity, mm2/s | 12 | |
3.0 |
Thermal Shock Resistance, points | 13 to 41 | |
38 |