Brinell Hardness 210
190 to 250
Elastic (Young's, Tensile) Modulus, GPa 190
190
Elongation at Break, % 20
21 to 23
Fatigue Strength, MPa 320
330 to 390
Poisson's Ratio 0.28
0.29
Shear Modulus, GPa 75
73
Tensile Strength: Ultimate (UTS), MPa 710
620 to 830
Tensile Strength: Yield (Proof), MPa 460
460 to 550

Thermal Properties

Latent Heat of Fusion, J/g 270
250
Maximum Temperature: Mechanical, °C 600
400
Melting Completion (Liquidus), °C 1460
1460
Melting Onset (Solidus), °C 1410
1420
Specific Heat Capacity, J/kg-K 470
470
Thermal Conductivity, W/m-K 26
52
Thermal Expansion, µm/m-K 13
13

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 9.2
7.3
Electrical Conductivity: Equal Weight (Specific), % IACS 11
8.4

Otherwise Unclassified Properties

Base Metal Price, % relative 6.5
2.3
Density, g/cm3 7.8
7.8
Embodied Carbon, kg CO2/kg material 2.1
1.8
Embodied Energy, MJ/kg 29
24 to 25
Embodied Water, L/kg 88
48

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 130
120 to 170
Resilience: Unit (Modulus of Resilience), kJ/m3 560
580 to 820
Stiffness to Weight: Axial, points 14
13
Stiffness to Weight: Bending, points 25
24
Strength to Weight: Axial, points 25
22 to 29
Strength to Weight: Bending, points 23
21 to 25
Thermal Diffusivity, mm2/s 6.9
14
Thermal Shock Resistance, points 20
18 to 24