MakeItFrom.com
Menu (ESC)

EN 1.8152 Steel vs. N07041 Nickel

EN 1.8152 steel belongs to the iron alloys classification, while N07041 nickel belongs to the nickel alloys. There are 13 material properties with values for both materials. Properties with values for just one material (18, in this case) are not shown.

For each property being compared, the top bar is EN 1.8152 steel and the bottom bar is N07041 nickel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
220
Tensile Strength: Ultimate (UTS), MPa 660 to 2010
1400

Thermal Properties

Melting Onset (Solidus), °C 1400
1320
Specific Heat Capacity, J/kg-K 480
450
Thermal Conductivity, W/m-K 47
11
Thermal Expansion, µm/m-K 13
12

Otherwise Unclassified Properties

Density, g/cm3 7.7
8.2

Common Calculations

Stiffness to Weight: Axial, points 13
15
Stiffness to Weight: Bending, points 25
25
Strength to Weight: Axial, points 24 to 72
47
Strength to Weight: Bending, points 22 to 46
34
Thermal Diffusivity, mm2/s 13
3.0
Thermal Shock Resistance, points 20 to 60
38