EN 2.4878 Nickel vs. N07041 Nickel
Both EN 2.4878 nickel and N07041 nickel are nickel alloys. There are 19 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.
For each property being compared, the top bar is EN 2.4878 nickel and the bottom bar is N07041 nickel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 200 | |
220 |
Elongation at Break, % | 13 to 17 | |
14 |
Fatigue Strength, MPa | 400 to 410 | |
540 |
Shear Strength, MPa | 750 to 760 | |
850 |
Tensile Strength: Ultimate (UTS), MPa | 1210 to 1250 | |
1400 |
Tensile Strength: Yield (Proof), MPa | 740 to 780 | |
1050 |
Thermal Properties
Melting Onset (Solidus), °C | 1320 | |
1320 |
Specific Heat Capacity, J/kg-K | 460 | |
450 |
Thermal Conductivity, W/m-K | 11 | |
11 |
Thermal Expansion, µm/m-K | 12 | |
12 |
Otherwise Unclassified Properties
Density, g/cm3 | 8.3 | |
8.2 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 150 to 180 | |
180 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 1370 to 1540 | |
2510 |
Stiffness to Weight: Axial, points | 13 | |
15 |
Stiffness to Weight: Bending, points | 24 | |
25 |
Strength to Weight: Axial, points | 41 to 42 | |
47 |
Strength to Weight: Bending, points | 31 | |
34 |
Thermal Diffusivity, mm2/s | 2.8 | |
3.0 |
Thermal Shock Resistance, points | 37 to 39 | |
38 |