EN AC-42100 Aluminum vs. 92-silver 8-tin-oxide

EN AC-42100 aluminum belongs to the aluminum alloys classification, while 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.

For each property being compared, the top bar is EN AC-42100 aluminum and the bottom bar is 92-silver 8-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 41
76 to 80
Elongation at Break, % 3.4 to 9.0
32 to 34
Resilience: Ultimate (Unit Rupture Work), MJ/m3 9.1 to 23
62 to 110
Tensile Strength: Ultimate (UTS), MPa 280 to 290
230 to 320
Tensile Strength: Yield (Proof), MPa 210 to 230
120 to 300