EN AC-44400 aluminum belongs to the aluminum alloys classification, while 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.

For each property being compared, the top bar is EN AC-44400 aluminum and the bottom bar is 92-silver 8-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 33
76 to 80
Elongation at Break, % 4.1
32 to 34
Resilience: Ultimate (Unit Rupture Work), MJ/m3 7.3
62 to 110
Tensile Strength: Ultimate (UTS), MPa 210
230 to 320
Tensile Strength: Yield (Proof), MPa 110
120 to 300