EN AC-45400 Aluminum vs. 90-silver 10-tin-oxide

EN AC-45400 aluminum belongs to the aluminum alloys classification, while 90-silver 10-tin-oxide belongs to the otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.

For each property being compared, the top bar is EN AC-45400 aluminum and the bottom bar is 90-silver 10-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 30
77 to 82
Elongation at Break, % 6.7
7.0 to 35
Resilience: Ultimate (Unit Rupture Work), MJ/m3 14
20 to 68
Tensile Strength: Ultimate (UTS), MPa 260
230 to 300
Tensile Strength: Yield (Proof), MPa 130
120 to 280