Electrical Conductivity: Equal Volume, % IACS | 27 | |
77 to 82 |
Elongation at Break, % | 1.1 | |
7.0 to 35 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 2.3 to 3.6 | |
20 to 68 |
Tensile Strength: Ultimate (UTS), MPa | 240 to 330 | |
230 to 300 |
Tensile Strength: Yield (Proof), MPa | 190 to 300 | |
120 to 280 |