EV31A magnesium belongs to the magnesium alloys classification, while C71520 copper-nickel belongs to the copper alloys. There are 23 material properties with values for both materials. Properties with values for just one material (11, in this case) are not shown. Please note that the two materials have significantly dissimilar densities. This means that additional care is required when interpreting the data, because some material properties are based on units of mass, while others are based on units of area or volume.

For each property being compared, the top bar is EV31A magnesium and the bottom bar is C71520 copper-nickel.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 44
140
Elongation at Break, % 3.5
10 to 45
Poisson's Ratio 0.27
0.33
Shear Modulus, GPa 17
51
Shear Strength, MPa 170
250 to 340
Tensile Strength: Ultimate (UTS), MPa 260
370 to 570
Tensile Strength: Yield (Proof), MPa 170
140 to 430

Thermal Properties

Maximum Temperature: Mechanical, °C 200
260
Melting Onset (Solidus), °C 590
1120
Specific Heat Capacity, J/kg-K 1000
400
Thermal Conductivity, W/m-K 86
32
Thermal Expansion, µm/m-K 27
15

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 18
5.7
Electrical Conductivity: Equal Weight (Specific), % IACS 90
5.8

Otherwise Unclassified Properties

Density, g/cm3 1.8
8.9

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 8.1
54 to 130
Resilience: Unit (Modulus of Resilience), kJ/m3 330
67 to 680
Stiffness to Weight: Axial, points 13
8.6
Stiffness to Weight: Bending, points 65
19
Strength to Weight: Axial, points 40
12 to 18
Strength to Weight: Bending, points 50
13 to 17
Thermal Diffusivity, mm2/s 47
8.9
Thermal Shock Resistance, points 16
12 to 19