Mechanical Properties
Compressive (Crushing) Strength, MPa | 21 | |
70 |
Elastic (Young's, Tensile) Modulus, GPa | 0.0075 | |
2.8 |
Elongation at Break, % | 440 | |
4.0 |
Tensile Strength: Ultimate (UTS), MPa | 16 | |
50 |
Thermal Properties
Maximum Temperature: Mechanical, °C | 130 | |
80 |
Thermal Expansion, µm/m-K | 650 | |
65 |
Otherwise Unclassified Properties
Density, g/cm3 | 1.5 | |
1.5 |
Common Calculations
Stiffness to Weight: Axial, points | 0.0029 | |
1.0 |
Stiffness to Weight: Bending, points | 4.5 | |
32 |
Strength to Weight: Axial, points | 3.0 | |
9.4 |
Strength to Weight: Bending, points | 9.5 | |