ECO Rubber vs. PEI
ECO rubber belongs to the thermoset elastomers (rubber) classification, while PEI belongs to the thermoplastics. There are 11 material properties with values for both materials. Properties with values for just one material (20, in this case) are not shown.
For each property being compared, the top bar is ECO rubber and the bottom bar is PEI.
Metric UnitsUS Customary Units
Mechanical Properties
Compressive (Crushing) Strength, MPa | 21 | |
140 to 180 |
Elastic (Young's, Tensile) Modulus, GPa | 0.0075 | |
3.4 to 5.6 |
Elongation at Break, % | 440 | |
3.0 to 34 |
Tensile Strength: Ultimate (UTS), MPa | 16 | |
110 to 160 |
Thermal Properties
Maximum Temperature: Mechanical, °C | 130 | |
170 |
Thermal Expansion, µm/m-K | 650 | |
20 to 53 |
Otherwise Unclassified Properties
Density, g/cm3 | 1.5 | |
1.3 to 1.5 |
Common Calculations
Stiffness to Weight: Axial, points | 0.0029 | |
1.5 to 2.1 |
Stiffness to Weight: Bending, points | 4.5 | |
39 |
Strength to Weight: Axial, points | 3.0 | |
24 to 30 |
Strength to Weight: Bending, points | 9.5 | |
40 to 44 |