Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 310
190
Elongation at Break, % 6.3
28
Poisson's Ratio 0.31
0.29
Shear Modulus, GPa 120
72
Tensile Strength: Ultimate (UTS), MPa 620
490
Tensile Strength: Yield (Proof), MPa 530
360

Thermal Properties

Latent Heat of Fusion, J/g 370
250
Specific Heat Capacity, J/kg-K 250
470
Thermal Expansion, µm/m-K 7.0
13

Otherwise Unclassified Properties

Density, g/cm3 10
7.9
Embodied Carbon, kg CO2/kg material 28
1.6
Embodied Energy, MJ/kg 330
21
Embodied Water, L/kg 360
52

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 37
120
Resilience: Unit (Modulus of Resilience), kJ/m3 450
340
Stiffness to Weight: Axial, points 17
13
Stiffness to Weight: Bending, points 22
24
Strength to Weight: Axial, points 17
17
Strength to Weight: Bending, points 16
17
Thermal Shock Resistance, points 21
14

Alloy Composition

Carbon (C), % 0 to 0.010
0 to 0.2
Copper (Cu), % 0
0.75 to 1.3
Iron (Fe), % 0 to 0.010
95.2 to 97.3
Manganese (Mn), % 0
0.4 to 1.1
Molybdenum (Mo), % 99.9 to 100
0
Nickel (Ni), % 0 to 0.0020
1.6 to 2.2
Nitrogen (N), % 0 to 0.0020
0
Oxygen (O), % 0 to 0.0015
0
Phosphorus (P), % 0
0 to 0.045
Silicon (Si), % 0 to 0.010
0
Sulfur (S), % 0
0 to 0.050