Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 0.4 | |
0.9 to 1.1 |
Elongation at Break, % | 350 | |
12 |
Tensile Strength: Ultimate (UTS), MPa | 37 | |
23 to 33 |
Thermal Properties
Maximum Temperature: Mechanical, °C | 75 | |
80 |
Melting Onset (Solidus), °C | 94 | |
150 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 Hz | 2.4 | |
2.2 to 2.3 |
Dielectric Strength (Breakdown Potential), kV/mm | 39 | |
21 to 22 |
Otherwise Unclassified Properties
Density, g/cm3 | 0.94 | |
0.9 |
Common Calculations
Stiffness to Weight: Axial, points | 0.24 | |
0.56 to 0.68 |
Stiffness to Weight: Bending, points | 26 | |
36 to 38 |
Strength to Weight: Axial, points | 11 | |
7.1 to 10 |
Strength to Weight: Bending, points | 26 | |
20 to 25 |