MakeItFrom.com
Menu (ESC)

Ionomer vs. UHMW-PE

Both ionomer and UHMW-PE are thermoplastics. There are 11 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.

For each property being compared, the top bar is ionomer and the bottom bar is UHMW-PE.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 0.4
0.8
Elongation at Break, % 350
400
Tensile Strength: Ultimate (UTS), MPa 37
49

Thermal Properties

Melting Onset (Solidus), °C 94
130
Vicat Softening Temperature, °C 72
75

Electrical Properties

Dielectric Constant (Relative Permittivity) At 1 Hz 2.4
2.2

Otherwise Unclassified Properties

Density, g/cm3 0.94
0.94

Common Calculations

Stiffness to Weight: Axial, points 0.24
0.47
Stiffness to Weight: Bending, points 26
33
Strength to Weight: Axial, points 11
14
Strength to Weight: Bending, points 26
32