IR Rubber vs. CSM Rubber
Both IR rubber and CSM rubber are thermoset elastomers (rubber). There are 7 material properties with values for both materials. Properties with values for just one material (6, in this case) are not shown.
For each property being compared, the top bar is IR rubber and the bottom bar is CSM rubber.
Metric UnitsUS Customary Units
Material Properties
Density, g/cm3 | 1.0 | |
1.2 |
Elongation at Break, % | 600 | |
400 |
Glass Transition Temperature, °C | -70 | |
0 |
Limiting Oxygen Index (LOI), % | 19 | |
25 |
Strength to Weight: Axial, points | 5.6 | |
2.1 |
Strength to Weight: Bending, points | 17 | |
8.0 |
Tensile Strength: Ultimate (UTS), MPa | 19 | |
9.0 |