Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 0.3 | |
1.1 |
Tensile Strength: Ultimate (UTS), MPa | 7.0 | |
24 |
Thermal Properties
Glass Transition Temperature, °C | -130 | |
30 |
Melting Onset (Solidus), °C | 110 | |
230 |
Specific Heat Capacity, J/kg-K | 2300 | |
1750 |
Thermal Conductivity, W/m-K | 0.36 | |
0.17 |
Thermal Expansion, µm/m-K | 220 | |
120 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 Hz | 2.3 | |
2.1 |
Otherwise Unclassified Properties
Density, g/cm3 | 0.92 | |
0.83 |
Common Calculations
Stiffness to Weight: Axial, points | 0.18 | |
0.74 |
Stiffness to Weight: Bending, points | 24 | |
41 |
Strength to Weight: Axial, points | 2.1 | |
8.0 |
Strength to Weight: Bending, points | 8.8 | |
22 |
Thermal Diffusivity, mm2/s | 0.17 | |
0.12 |
Thermal Shock Resistance, points | 7.6 | |
13 |