Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 180
190
Elongation at Break, % 11
21 to 27
Fatigue Strength, MPa 450
200 to 320
Poisson's Ratio 0.3
0.28 to 0.29
Shear Modulus, GPa 70
73 to 75
Tensile Strength: Ultimate (UTS), MPa 1340
540 to 710
Tensile Strength: Yield (Proof), MPa 930
270 to 460

Thermal Properties

Latent Heat of Fusion, J/g 290
250 to 270
Maximum Temperature: Mechanical, °C 920
410 to 600
Melting Completion (Liquidus), °C 1430
1450 to 1460
Melting Onset (Solidus), °C 1380
1410 to 1420
Specific Heat Capacity, J/kg-K 460
470
Thermal Conductivity, W/m-K 11
26 to 50
Thermal Expansion, µm/m-K 8.6
13

Otherwise Unclassified Properties

Base Metal Price, % relative 50
2.4 to 7.0
Density, g/cm3 8.3
7.8
Embodied Carbon, kg CO2/kg material 9.3
1.5 to 2.1
Embodied Energy, MJ/kg 140
20 to 28
Embodied Water, L/kg 170
47 to 87

Common Calculations

PREN (Pitting Resistance) 4.2
2.5 to 13
Resilience: Ultimate (Unit Rupture Work), MJ/m3 140
110 to 130
Resilience: Unit (Modulus of Resilience), kJ/m3 2340
190 to 570
Stiffness to Weight: Axial, points 12
13 to 14
Stiffness to Weight: Bending, points 23
24 to 25
Strength to Weight: Axial, points 45
19 to 25
Strength to Weight: Bending, points 33
19 to 23
Thermal Diffusivity, mm2/s 2.9
6.9 to 14
Thermal Shock Resistance, points 61
16 to 20