Nickel Beryllium 360 vs. AWS ERNiCrMo-10
Both nickel beryllium 360 and AWS ERNiCrMo-10 are nickel alloys. There are 19 material properties with values for both materials. Properties with values for just one material (10, in this case) are not shown.
For each property being compared, the top bar is nickel beryllium 360 and the bottom bar is AWS ERNiCrMo-10.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 200 | |
220 |
Elongation at Break, % | 1.0 to 30 | |
28 |
Poisson's Ratio | 0.3 | |
0.29 |
Shear Modulus, GPa | 77 | |
84 |
Tensile Strength: Ultimate (UTS), MPa | 780 to 1860 | |
790 |
Thermal Properties
Melting Completion (Liquidus), °C | 1330 | |
1550 |
Melting Onset (Solidus), °C | 1200 | |
1490 |
Specific Heat Capacity, J/kg-K | 460 | |
420 |
Thermal Conductivity, W/m-K | 48 | |
10 |
Thermal Expansion, µm/m-K | 14 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 5.0 | |
1.5 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 5.4 | |
1.5 |
Otherwise Unclassified Properties
Density, g/cm3 | 8.3 | |
8.9 |
Common Calculations
Stiffness to Weight: Axial, points | 13 | |
14 |
Stiffness to Weight: Bending, points | 24 | |
23 |
Strength to Weight: Axial, points | 26 to 62 | |
25 |
Strength to Weight: Bending, points | 23 to 41 | |
21 |
Thermal Diffusivity, mm2/s | 13 | |
2.7 |
Thermal Shock Resistance, points | 19 to 46 | |
21 |