ACM Rubber vs. PC
ACM rubber belongs to the thermoset elastomers (rubber) classification, while PC belongs to the thermoplastics. There are 6 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.
For each property being compared, the top bar is ACM rubber and the bottom bar is PC.
Metric UnitsUS Customary Units
Material Properties
Density, g/cm3 | 1.3 | |
1.2 to 1.4 |
Elongation at Break, % | 280 | |
3.5 to 110 |
Glass Transition Temperature, °C | -40 | |
150 |
Strength to Weight: Axial, points | 2.7 | |
15 to 30 |
Strength to Weight: Bending, points | 9.3 | |
30 to 45 |
Tensile Strength: Ultimate (UTS), MPa | 13 | |
66 to 160 |