Material Properties
Elongation at Break, % | 2.8 to 46 | |
380 |
Glass Transition Temperature, °C | 50 | |
-45 |
Limiting Oxygen Index (LOI), % | 26 | |
26 |
Maximum Temperature: Autoignition, °C | 460 | |
410 |
Maximum Temperature: Decomposition, °C | 410 | |
350 |
Tensile Strength: Ultimate (UTS), MPa | 60 to 240 | |
11 |