Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 1.1 to 16 | |
3.6 |
Elongation at Break, % | 2.5 to 67 | |
26 |
Flexural Modulus, GPa | 1.2 to 14 | |
4.7 |
Flexural Strength, MPa | 40 to 230 | |
130 |
Tensile Strength: Ultimate (UTS), MPa | 35 to 210 | |
95 |
Thermal Properties
Glass Transition Temperature, °C | 40 | |
220 |
Maximum Temperature: Autoignition, °C | 430 | |
580 |
Maximum Temperature: Decomposition, °C | 430 | |
560 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 MHz | 3.3 to 5.0 | |
3.4 |
Dielectric Strength (Breakdown Potential), kV/mm | 10 to 30 | |
16 |
Otherwise Unclassified Properties
Limiting Oxygen Index (LOI), % | 24 | |
38 |