Metric UnitsUS Customary Units
Material Properties
Density, g/cm3 | 1.4 | |
0.94 |
Dielectric Constant (Relative Permittivity) At 1 Hz | 3.5 | |
2.4 |
Dielectric Strength (Breakdown Potential), kV/mm | 15 | |
39 |
Elastic (Young's, Tensile) Modulus, GPa | 2.7 | |
0.4 |
Elongation at Break, % | 40 | |
350 |
Stiffness to Weight: Axial, points | 1.1 | |
0.24 |
Stiffness to Weight: Bending, points | 34 | |
26 |
Strength to Weight: Axial, points | 17 | |
11 |
Strength to Weight: Bending, points | 31 | |
26 |
Tensile Strength: Ultimate (UTS), MPa | 83 | |
37 |