Material Properties
Dielectric Constant (Relative Permittivity) At 1 MHz | 3.2 to 3.7 | |
3.6 to 4.7 |
Dielectric Strength (Breakdown Potential), kV/mm | 30 to 33 | |
15 to 30 |
Elastic (Young's, Tensile) Modulus, GPa | 3.4 to 5.6 | |
1.0 to 16 |
Electrical Resistivity Order of Magnitude, 10x Ω-m | 14 to 15 | |
7.0 to 13 |
Elongation at Break, % | 3.0 to 34 | |
2.5 to 50 |
Flexural Modulus, GPa | 3.4 to 5.9 | |
0.9 to 14 |
Flexural Strength, MPa | 140 to 210 | |
50 to 350 |
Tensile Strength: Ultimate (UTS), MPa | 110 to 160 | |
120 to 250 |