PPSU vs. PA 6
Both PPSU and PA 6 are thermoplastics. There are 11 material properties with values for both materials. Properties with values for just one material (22, in this case) are not shown.
For each property being compared, the top bar is PPSU and the bottom bar is PA 6.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 3.6 | |
1.1 to 16 |
Elongation at Break, % | 26 | |
2.5 to 67 |
Flexural Modulus, GPa | 4.7 | |
1.2 to 14 |
Flexural Strength, MPa | 130 | |
40 to 230 |
Tensile Strength: Ultimate (UTS), MPa | 95 | |
35 to 210 |
Thermal Properties
Glass Transition Temperature, °C | 220 | |
40 |
Maximum Temperature: Autoignition, °C | 580 | |
430 |
Maximum Temperature: Decomposition, °C | 560 | |
430 |
Electrical Properties
Dielectric Constant (Relative Permittivity) At 1 MHz | 3.4 | |
3.3 to 5.0 |
Dielectric Strength (Breakdown Potential), kV/mm | 16 | |
10 to 30 |
Otherwise Unclassified Properties
Limiting Oxygen Index (LOI), % | 38 | |
24 |