Material Properties
Density, g/cm3 | 1.1 | |
1.2 to 1.6 |
Elongation at Break, % | 30 | |
2.0 to 52 |
Flexural Modulus, GPa | 2.3 to 2.4 | |
2.7 to 14 |
Flexural Strength, MPa | 95 to 110 | |
110 to 200 |
Heat Deflection Temperature At 1.82 MPa (264 psi), °C | 120 | |
180 to 200 |
Specific Heat Capacity, J/kg-K | 1400 | |
910 to 1000 |
Strength to Weight: Axial, points | 14 to 17 | |
16 to 25 |
Strength to Weight: Bending, points | 29 to 33 | |
30 to 40 |
Tensile Strength: Ultimate (UTS), MPa | 57 to 69 | |
70 to 140 |