MakeItFrom.com
Menu (ESC)

AU vs. POM-H

AU belongs to the thermoset elastomers (rubber) classification, while POM-H belongs to the thermoplastics. There are 3 material properties with values for both materials. Properties with values for just one material (10, in this case) are not shown.

For each property being compared, the top bar is AU and the bottom bar is POM-H.

Metric UnitsUS Customary Units

Material Properties

Elongation at Break, % 580
7.0 to 55
Specific Heat Capacity, J/kg-K 1760
1250 to 1460
Tensile Strength: Ultimate (UTS), MPa 39
60 to 67