AU vs. UP
AU belongs to the thermoset elastomers (rubber) classification, while UP belongs to the thermoset plastics. There are 5 material properties with values for both materials. Properties with values for just one material (14, in this case) are not shown.
For each property being compared, the top bar is AU and the bottom bar is UP.
Metric UnitsUS Customary Units
Material Properties
Elongation at Break, % | 580 | |
1.0 |
Glass Transition Temperature, °C | -50 | |
60 |
Specific Heat Capacity, J/kg-K | 1760 | |
1200 |
Tensile Strength: Ultimate (UTS), MPa | 39 | |
30 |
Thermal Conductivity, W/m-K | 0.19 | |
0.7 |