SAE-AISI 1541 steel belongs to the iron alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.

For each property being compared, the top bar is SAE-AISI 1541 steel and the bottom bar is 88-silver 12-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 7.1
84 to 86
Elongation at Break, % 11 to 17
9.0 to 37
Resilience: Ultimate (Unit Rupture Work), MJ/m3 78 to 100
24 to 70
Shear Strength, MPa 440 to 480
150 to 160
Tensile Strength: Ultimate (UTS), MPa 720 to 790
230 to 280
Tensile Strength: Yield (Proof), MPa 390 to 680
110 to 260