SAE-AISI 1547 Steel vs. 88-silver 12-tin-oxide
SAE-AISI 1547 steel belongs to the iron alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.
For each property being compared, the top bar is SAE-AISI 1547 steel and the bottom bar is 88-silver 12-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 7.1 | |
84 to 86 |
Elongation at Break, % | 11 to 17 | |
9.0 to 37 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 80 to 110 | |
24 to 70 |
Shear Strength, MPa | 440 to 480 | |
150 to 160 |
Tensile Strength: Ultimate (UTS), MPa | 740 to 800 | |
230 to 280 |
Tensile Strength: Yield (Proof), MPa | 400 to 690 | |
110 to 260 |