MakeItFrom.com
Menu (ESC)

SAE-AISI 4028 Steel vs. 88-silver 12-tin-oxide

SAE-AISI 4028 steel belongs to the iron alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.

For each property being compared, the top bar is SAE-AISI 4028 steel and the bottom bar is 88-silver 12-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 7.1
84 to 86
Elongation at Break, % 14 to 23
9.0 to 37
Resilience: Ultimate (Unit Rupture Work), MJ/m3 81 to 95
24 to 70
Shear Strength, MPa 310 to 380
150 to 160
Tensile Strength: Ultimate (UTS), MPa 490 to 630
230 to 280
Tensile Strength: Yield (Proof), MPa 260 to 520
110 to 260