Metric UnitsUS Customary Units
Material Properties
Density, g/cm3 | 1.4 to 1.5 | |
1.1 |
Elastic (Young's, Tensile) Modulus, GPa | 3.7 to 20 | |
2.6 |
Elongation at Break, % | 1.8 to 7.5 | |
6.0 |
Glass Transition Temperature, °C | 260 | |
100 |
Specific Heat Capacity, J/kg-K | 970 to 1100 | |
1300 |
Stiffness to Weight: Axial, points | 1.5 to 7.9 | |
1.3 |
Stiffness to Weight: Bending, points | 37 to 64 | |
43 |
Strength to Weight: Axial, points | 22 to 42 | |
14 |
Strength to Weight: Bending, points | 36 to 57 | |
30 |
Tensile Strength: Ultimate (UTS), MPa | 110 to 220 | |
55 |